1
www.masterbond.com Hackensack, NJ 07601, USA +1.201.343.8983 ∙ [email protected] CAN YOUR EPOXY ADHESIVE GO LOW? Epoxy System EP42HT-2LTE Features an ultra low coefficient of thermal expansion ADHESIVE SPREADS EVENLY CTE 9-12 X 10 -6 in/in/°C LOW SHRINKAGE UPON CURE Linear <0.01% Volumetric <0.1% Elongation <5% HIGH DIMENSIONAL STABILITY From -60 to +300°F HARDNESS >85 Shore D HIGH TENSILE MODULUS 400,000-500,000 psi

Can Your Epoxy Adhesive Go Low?

Embed Size (px)

Citation preview

Page 1: Can Your Epoxy Adhesive Go Low?

www.masterbond.com

Hackensack, NJ 07601, USA+1.201.343.8983 ∙ [email protected]

CAN YOUR EPOXY

ADHESIVE GO LOW?Epoxy System EP42HT-2LTEFeatures an ultra low coefficient

of thermal expansion

ADHESIVE SPREADS EVENLY

CTE 9-12 X 10-6 in/in/°C

LOW SHRINKAGE UPON CURELinear <0.01%Volumetric <0.1%

Elongation <5%

HIGH DIMENSIONAL STABILITY

From -60 to +300°F

HARDNESS

>85 Shore D

HIGH TENSILE MODULUS

400,000-500,000 psi