Cu-c2 (Cu-OFE) Chemical compound (NFA 51-050) Type Cu mini in % Max. electrictal resistivity at 20 °C at the annealing state (C % IACS min) Free from oxygen, high purity 99,95 1,707 μOhm.cm (100% IACS) Mechanical characteristics of rolled products (NFA 51-100): State Rm in N/mm² A % mini Hardness HV O mini 200 30 65 H11 from 230 to 280 20 from 55 to 80 H12 from 260 to 320 10 from 75 to 105 H14 mini 300 - mini 100 Physical characteristics of rolled products (NFA 51-100): Melting temperature (liquidus) in °C Temperature of incipient melting (solidus) en °C Mass volume in g/cm 3 Electrical resistivity at 20° C in μOhm.cm Conductivity in % IACS Heat conductivity at 20°C in W/m.K 1083 1083 8,94 1,682 to 1,7241 100 to 102,5 400 to 412 Page 1 of 1 cuc2 14/06/2013 http://www.euralliage.com/cuc2_english.htm

Cu C2 (Cu OFE) Specifications

Embed Size (px)

Citation preview

Page 1: Cu C2 (Cu OFE) Specifications

Cu-c2 (Cu-OFE)

Chemical compound (NFA 51-050)

Type Cu mini in % Max. electrictal resistivity at 20 °C at the

annealing state (C % IACS min) Free from oxygen, high purity 99,95 1,707 µOhm.cm (100% IACS)

Mechanical characteristics of rolled products (NFA 51-100):

State Rm in N/mm² A % mini Hardness HV O mini 200 30 65

H11 from 230 to 280 20 from 55 to 80 H12 from 260 to 320 10 from 75 to 105 H14 mini 300 - mini 100

Physical characteristics of rolled products (NFA 51-100):

Melting temperature

(liquidus) in °C

Temperature of incipient melting (solidus) en °C

Mass volume in g/cm3

Electrical resistivity at 20°C in µOhm.cm

Conductivity in % IACS

Heat conductivity at 20°C in W/m.K

1083 1083 8,94 1,682 to 1,7241 100 to 102,5 400 to 412