with the indentation test specified by DIN 30670 (Push for 24 hours under 9.8 N /mm2 of pressure...
9
with the indentation test specified by DIN 30670 (Push for 24 hours under 9.8 N /mm2 of pressure with a needle of 2.5 mm2 in cross-section area ) Figure 3 shows the indentation resistance