Welding Defects Eurotech Now inteducing Welding Defects. Welding Defect is any type of flaw in the object which requires welding. Seven type of Welding Defect Seven type of Common weld defects include: 1. Lack of fusion 2. Lack of penetration or excess penetration 3. Porosity 4. Inclusions 5. Cracking 6. Undercut 7. Lamellar tearing Any of these defects are potentially disastrous as they can all give rise to high stress intensities which may result in sudden unexpected failure below the design load or in the case of cyclic loading, failure after fewer load cycles than predicted. - PowerPoint PPT Presentation
Citation preview
Welding Defects
www.eurotechworld.net
https://www.eurotechworld.net/weldingtrainings
Meaning:A welding defect is any type of flaw in a welding job that compromises the use and function of the object that received the welding.
www.eurotechworld.net
Types of Welding defectsLack of FusionUndercuttingPinholesCrackingMisalignmentGas InclusionsPorosityCratersOverlap
www.eurotechworld.net
Types of Welding defectsLamellar TearingReheat crackingRoot and Toe Cracks
www.eurotechworld.net
Lack of FusionLack of fusion is the poor adhesion of the
weld bead to the base metal. If the weld heat was not high enough, the metals being welded together may not have become molten during the welding process and the two pieces did not join.
www.eurotechworld.net
Under CuttingWelding along a line or using an arc
voltage that is too low can produce a groove or a slight ditch in the metal right along the weld line. This is known as undercutting.
www.eurotechworld.net
PinholesWelding defect caused by the high
welding temperatures is known as Pinholes. If the temperature of arc making of the weld is very high, then tiny holes resembling pin holes may appear on the surface of the weld.
www.eurotechworld.net
CrackingThis defect typically occurs because the
welder was using the wrong type of wire electrode to make the weld. A combination of poor design and inappropriate procedure may result in high residual stresses and cracking.
www.eurotechworld.net
MisalignmentThis type defect is generally caused
by a setup/fit up problem, or trying to join plates of different thickness.
www.eurotechworld.net
Gas InclusionsGas inclusions is also a defect that includes
porosity, blow holes, and pipes. The cause for gas inclusions is the entrapment of gas within the solidified weld.
It can be from any of the following causes: high sulphur content in the electrode, excessive moisture from the electrode or wrong welding.
www.eurotechworld.net
CratersCrater cracks occur when a crater is not
filled before the arc is broken. This causes the outer edges of the crater to cool more quickly than the crater, which creates sufficient stresses to form a crack.
www.eurotechworld.net
OverlappingThe protrusion of weld metal beyond the
weld toe or weld root. It is caused by poor welding techniques and can generally be overcome by an improved weld procedure. The overlap can be repaired by grinding off excess weld metal and surface grinding smoothly to the base metal.
www.eurotechworld.net
Lamellar TearingLamellar tearing is a type of defect that is
most likely to occur below a welded joint at points of high stress concentration. Lamellar tearing is caused mainly by sulphur inclusions in the material. Other causes include an excess of hydrogen in the alloy.
This defect can be removed by keeping the amount of sulfur in the steel alloy below 0.005%
www.eurotechworld.net
Root and Toe CracksA root crack is the crack formed by the short
bead at the root beginning of the welding, low current at the beginning and due to improper filler material used for welding.
Major reason for happening of these types of cracks is hydrogen embrittlement.
These types of defects can be eliminated using high current at the starting and proper filler material.
www.eurotechworld.net
Reheat CrackingReheat cracking is a type of cracking that occurs
in HSLA steels, particularly chromium, molybdenum and vanadium steels, during post heating.
It is caused by the poor creep ductility of the heat affected zone.
It can be eliminated by heat treating first with a low temperature soak and then with a rapid heating to high temperatures, grinding or peening the weld toes