6
WATERPROOFING SPECIFICATIONS AND METHODOLOGIES SWIMMING POOL 101 Concrete Waterproofing and Durability Enhancement Using DPC Supershield Crystalline Technology www.supershieldglobal.com SWIMMING POOL - PREREQUISITE FOR SUPERSHIELD WATERPROOFING TREATMENT l The SWIMMING POOL that is to be treated should be minimum 7 days old. SUPERSHIELD SPECIFICATION AND APPLICATION METHODOLOGY Provide, mix and brush apply two coats of SUPERSHIELD CRYSTALGUARD, single compound Deep Penetrating Capillary (DPC) waterproofing system that generates a non-soluble crystalline formation of dendritic fibers within the pores and capillary tracts of the concrete @ 1.5 Kg/m² for two coats on the walls and the floor area of the Swimming pool. 1) Surface preparation - The concrete substrate that to be applied with SUPERSHIELD CRYSTALGUARD must be free from foreign materials and to be micro cleaned by mechanical means like wire brushing or vacuum cleaning. 2) Pre-wetting - Concrete surface must be thoroughly saturated with clean water prior to the coating to ensure moisture presence inside the pores and capillaries and remove any excess water and ensure surface is touch dry while coating. 3) Mixing of CRYSTALGUARD - Mix SUPERSHIELD CRYSTALGUARD powder with clean water to form a slurry consistency with 5 parts of powder and 2 parts of water. 4) Application of CRYSTALGUARD - Apply the first coat of SUPERSHIELD CRYSTALGUARD as a slurry consistency on the concrete surface. Concrete Substrate Application Methodology TWO COATS OF CRYSTALGUARD @ 1.5 Kg/m² SWIMMING POOL - 101 Page 1 of 3 SWIMMING POOL SUPERSHIELD CRYSTALGUARD FIRST COATING SUPERSHIELD CRYSTALGUARD SECOND COATING Construction Joint

SWIMMING POOL - Supershield

  • Upload
    others

  • View
    8

  • Download
    0

Embed Size (px)

Citation preview

Page 1: SWIMMING POOL - Supershield

WATERPROOFING SPECIFICATIONS AND METHODOLOGIES

SWIMMING POOL 101

Concrete Waterproofing and Durability Enhancement Using DPC Supershield Crystalline Technology

www.supershieldglobal.com

SWIMMING POOL - PREREQUISITE FOR SUPERSHIELD WATERPROOFING TREATMENT

l The SWIMMING POOL that is to be treated should be minimum 7 days old.

SUPERSHIELD SPECIFICATION AND APPLICATION METHODOLOGY

Provide, mix and brush apply two coats of SUPERSHIELD CRYSTALGUARD, single compound Deep Penetrating

Capillary (DPC) waterproofing system that generates a non-soluble crystalline formation of dendritic fibers within

the pores and capillary tracts of the concrete @ 1.5 Kg/m² for two coats on the walls and the floor area of the

Swimming pool.

1) Surface preparation - The concrete substrate that to be applied with SUPERSHIELD

CRYSTALGUARD must be free from foreign materials and to be micro cleaned by mechanical means like

wire brushing or vacuum cleaning.

2) Pre-wetting - Concrete surface must be thoroughly saturated with clean water prior to the coating to

ensure moisture presence inside the pores and capillaries and remove any excess water and ensure

surface is touch dry while coating.

3) Mixing of CRYSTALGUARD - Mix SUPERSHIELD CRYSTALGUARD powder with clean water to form a

slurry consistency with 5 parts of powder and 2 parts of water.

4) Application of CRYSTALGUARD - Apply the first coat of SUPERSHIELD CRYSTALGUARD as a slurry

consistency on the concrete surface.

Concrete Substrate

Application Methodology

TWO COATS OF CRYSTALGUARD @ 1.5 Kg/m²

SWIMMING POOL - 101 Page 1 of 3

SWIMMING POOL

SUPERSHIELD CRYSTALGUARD FIRST COATING

SUPERSHIELDCRYSTALGUARD SECOND COATING

Construction Joint

Page 2: SWIMMING POOL - Supershield

5) Second coat of CRYSTALGUARD - Apply the second coat of SUPERSHIELD CRYSTALGUARD as a

slurry consistency on the first coat after a minimum of 4 hours gap.

l The SUPERSHIELD CRYSTALGUARD coating should be cured with a misty fog spray of clean water, 24 hours

after the application and to be kept moist for minimum 3 days.

Cracks, horizontal, vertical joint sealing, tie hole, pipe penetrations, construction joints, expansion joints and

other defects in the concrete that to be waterproofed should be treated as per the SUPERSHIELD specification

and application methodology.

Crystalline waterproofing system should meet or exceed the performance requirements as specified herein.

l Crystalline Penetration : Crystallizing capability of waterproofing material shall be evidenced by

independent SEM (Scanning Electron Microscope) photographs documenting penetration of needle like

crystal formation deep within concrete.

l Self-healing capability and permeability resistance : Independent testing performed according to U.S. Army

Corps of Engineers CRD-C48-73 "Permeability of Concrete".

l Testing on the effectiveness of coating from negative side of concrete : Independent testing that

demonstrates the capability of the coating to seal the leakage/dampness from negative side.

l Resistance to chloride ion penetration : Independent testing performed according to ASTM C 1202-03

should exhibit a resistance of 100% better than that of the untreated specimen.

l Potable Water Approval : Independent testing shall be performed according to EN or NSF Standard 61, and

approval for use of waterproofing material on structures holding potable water shall be evidenced.

A) Manufacturer : Manufacturer should publish a third party product quality assurance certificate from a notified

body with continuous surveillance audit or CE certificate with FPC (Factory Production Control) as per the

harmonized standard EN to prove that the facility from where the material is produced for the project has

undergone the required testing and extensive inspection and is under continuous surveillance by a notified body

appointed by the European union as per the European norms for the system. Manufacturers who cannot provide

the performance test data specified herein and FPC certificate shall not be considered for the project.

B) Applicator : Waterproofing applicator shall be experienced in the installation of cementitious crystalline

waterproofing materials and shall be approved by the manufacturer in writing.

Curing

Watch Points

Performance Criteria

Quality Assurance

www.supershieldglobal.com SWIMMING POOL - 101 Page 2 of 3

WATERPROOFING SPECIFICATIONS AND METHODOLOGIES

SWIMMING POOL 101

Concrete Waterproofing and Durability Enhancement Using DPC Supershield Crystalline Technology

TWO COATS OF CRYSTALGUARD @ 1.5 Kg/m²

Page 3: SWIMMING POOL - Supershield

Warranty

Submittals

A) Manufacturer's Warranty : Manufacturer shall provide standard product warranty executed by authorised

company official.

B) Applicator's Warranty : Applicator shall warrant the waterproofing installation against defects caused by faulty

workmanship or materials for a period of (specify term) years from Date of Substantial Completion. The warranty

will cover the surfaces treated and will bind the applicator to repair, at his expense, any and all leaks through the

treated surfaces which are not due to structural weaknesses or other causes beyond applicator's control such as

fire, earthquake and cyclone.

Product data sheets, Application guidelines, Material safety data sheet, CE certificate, Summary of test reports.

www.supershieldglobal.com SWIMMING POOL - 101 Page 3 of 3

WATERPROOFING SPECIFICATIONS AND METHODOLOGIES

SWIMMING POOL 101

Concrete Waterproofing and Durability Enhancement Using DPC Supershield Crystalline Technology

TWO COATS OF CRYSTALGUARD @ 1.5 Kg/m²

Page 4: SWIMMING POOL - Supershield

www.supershieldglobal.com

SWIMMING POOL - PREREQUISITE FOR SUPERSHIELD WATERPROOFING TREATMENT

l The SWIMMING POOL that is to be treated should be minimum 7 days old.

SUPERSHIELD SPECIFICATION AND APPLICATION METHODOLOGY

Provide, mix and brush apply one coat of SUPERSHIELD CRYSTALGUARD, single compound Deep Penetrating

Capillary (DPC) waterproofing system @ 0.75 Kg/m² and one coat of SUPERSHIELD CRYSTALGUARD ULTIMA,

single compound highly concentrated crystalline coating as a top coat that generates a non-soluble crystalline

formation of dendritic fibers within the pores and capillary tracts of the concrete with hard surface finish @ 0.75

Kg/m² on the wall and the floor area of the Swimming Pool.

1) Surface preparation - The concrete substrate that is to be applied with SUPERSHIELD

CRYSTALGUARD /ULTIMA must be free from foreign materials and to be micro cleaned by mechanical

means like wire brushing or vacuum cleaning.

2) Pre-wetting - Concrete surface must be thoroughly saturated with clean water prior to the coating to

ensure moisture presence inside the pores and capillaries and remove any excess water to ensure

surface is touch dry while coating.

3) Mixing of CRYSTALGUARD - Mix SUPERSHIELD CRYSTALGUARD powder with clean water to form a

slurry consistency with 5 parts of powder and 2 parts of water.

Concrete Substrate

Application Methodology

WATERPROOFING SPECIFICATIONS AND METHODOLOGIES

2 ONE COAT OF CRYSTALGUARD & ONE COAT OF CRYSTALGUARD ULTIMA @ 1.5 Kg/m

SWIMMING POOL 102

SWIMMING POOL - 102 Page 1 of 3

SWIMMING POOL

SUPERSHIELDCRYSTALGUARDCOATING

SUPERSHIELDCRYSTALGUARD ULTIMACOATING

Construction Joint

Concrete Waterproofing and Durability Enhancement Using DPC Supershield Crystalline Technology

Page 5: SWIMMING POOL - Supershield

4) Application of CRYSTALGUARD - Apply one coat of SUPERSHIELD CRYSTALGUARD as a slurry

consistency on to the concrete surface.

5) Mixing of CRYSTALGUARD ULTIMA - Mix SUPERSHIELD CRYSTALGUARD ULTIMA powder with

clean water to form a slurry consistency withf 5 parts of powder and 2 parts of water.

6) Application of CRYSTALGUARD ULTIMA - Apply one coat of SUPERSHIELD CRYSTALGUARD

ULTIMA as a slurry consistency on the CRYSTALGUARD coating minimum after 4 hours gap as a top

coating.

Cracks, horizontal, vertical joint sealing, tie hole, pipe penetrations, construction joints, expansion joints and

other defects in the concrete that to be waterproofed should be treated as per the SUPERSHIELD specification

and application methodology.

Crystalline waterproofing system should meet or exceed the performance requirements as specified herein.

l Crystalline Penetration : Crystallizing capability of waterproofing material shall be evidenced by

independent SEM (Scanning Electron Microscope) photographs documenting penetration of needle like

crystal formation deep within concrete.

l Self-healing capability and permeability resistance : Independent testing performed according to U.S. Army

Corps of Engineers CRD-C48-73 "Permeability of Concrete".

l Testing on the effectiveness of coating from negative side of concrete : Independent testing that

demonstrates the capability of the coating to seal the leakage/dampness from negative side.

l Resistance to chloride ion penetration : Independent testing performed according to ASTM C 1202-03

should exhibit a resistance of 100% better than that of the untreated specimen.

l Potable Water Approval : Independent testing shall be performed according to EN or NSF Standard 61, and

approval for use of waterproofing material on structures holding potable water shall be evidenced.

A) Manufacturer : Manufacturer should publish a third party product quality assurance certificate from a notified

body with continuous surveillance audit or CE certificate with FPC (Factory Production Control) as the per the

harmonized standard EN to prove that the facility from where the material is produced for the project has

Curing

Watch Points

Performance Criteria

Quality Assurance

l The SUPERSHIELD CRYSTALGUARD/ ULTIMA coating should be cured with a misty fog spray of clean water,

24 hours after the application and to be kept moist for minimum 3 days.

www.supershieldglobal.com SWIMMING POOL - 102 Page 2 of 3

WATERPROOFING SPECIFICATIONS AND METHODOLOGIES

2 ONE COAT OF CRYSTALGUARD & ONE COAT OF CRYSTALGUARD ULTIMA @ 1.5 Kg/m

SWIMMING POOL 102

Concrete Waterproofing and Durability Enhancement Using DPC Supershield Crystalline Technology

Page 6: SWIMMING POOL - Supershield

undergone the required testing and extensive inspection and is under continuous surveillance by a notified body

appointed by the European union as per the European norms for the system. Manufacturers who cannot provide

the performance test data specified herein and FPC certificate shall not be considered for the project.

B) Applicator : Waterproofing applicator shall be experienced in the installation of cementitious crystalline

waterproofing materials and shall be approved by the manufacturer in writing.

A) Manufacturer's Warranty : Manufacturer shall provide standard product warranty executed by authorised

company official.

B) Applicator's Warranty : Applicator shall warrant the waterproofing installation against defects caused by

faulty workmanship or materials for a period of (specify term) years from Date of Substantial Completion. The

warranty will cover the surfaces treated and will bind the applicator to repair, at his expense, any and all leaks

through the treated surfaces which are not due to structural weaknesses or other causes beyond applicator's

control such as fire, earthquake and cyclone.

Product data sheets, Application guidelines, Material safety data sheet, CE certificate, Summary of test reports.

Warranty

Submittals

www.supershieldglobal.com SWIMMING POOL - 102 Page 3 of 3

WATERPROOFING SPECIFICATIONS AND METHODOLOGIES

2 ONE COAT OF CRYSTALGUARD & ONE COAT OF CRYSTALGUARD ULTIMA @ 1.5 Kg/m

SWIMMING POOL 102

Concrete Waterproofing and Durability Enhancement Using DPC Supershield Crystalline Technology