SHEET RUBBER
HEAT AND CHEMICAL WELDING
Page 1 of 17
http://www.american-biltrite.com | [email protected]
1-800-437-8743 6090-A (2019-05-21)
Heat Welding of Sheet Rubber
Coving of Internal Corner
Trim and Fit the Piece
SHEET RUBBER
HEAT AND CHEMICAL WELDING
Page 2 of 17
http://www.american-biltrite.com | [email protected]
1-800-437-8743 6090-A (2019-05-21)
Trim the Corner
Adjust the Other Side
SHEET RUBBER
HEAT AND CHEMICAL WELDING
Page 3 of 17
http://www.american-biltrite.com | [email protected]
1-800-437-8743 6090-A (2019-05-21)
Cut and Fit
Weld In Place
SHEET RUBBER
HEAT AND CHEMICAL WELDING
Page 4 of 17
http://www.american-biltrite.com | [email protected]
1-800-437-8743 6090-A (2019-05-21)
Shave Off the Surplus
Finished Inside Weld
SHEET RUBBER
HEAT AND CHEMICAL WELDING
Page 5 of 17
http://www.american-biltrite.com | [email protected]
1-800-437-8743 6090-A (2019-05-21)
Coving of External Corner
Fitting the Pieces Together
SHEET RUBBER
HEAT AND CHEMICAL WELDING
Page 6 of 17
http://www.american-biltrite.com | [email protected]
1-800-437-8743 6090-A (2019-05-21)
Welding
Trimming
SHEET RUBBER
HEAT AND CHEMICAL WELDING
Page 7 of 17
http://www.american-biltrite.com | [email protected]
1-800-437-8743 6090-A (2019-05-21)
Final Look
Or You Can also Do It This Way
SHEET RUBBER
HEAT AND CHEMICAL WELDING
Page 8 of 17
http://www.american-biltrite.com | [email protected]
1-800-437-8743 6090-A (2019-05-21)
Bring Sheet up to the Corner
Cut and Adjust to the Corner
SHEET RUBBER
HEAT AND CHEMICAL WELDING
Page 9 of 17
http://www.american-biltrite.com | [email protected]
1-800-437-8743 6090-A (2019-05-21)
Weld
Trim
SHEET RUBBER
HEAT AND CHEMICAL WELDING
Page 10 of 17
http://www.american-biltrite.com | [email protected]
1-800-437-8743 6090-A (2019-05-21)
Final Touch
SHEET RUBBER
HEAT AND CHEMICAL WELDING
Page 11 of 17
http://www.american-biltrite.com | [email protected]
1-800-437-8743 6090-A (2019-05-21)
Final look of Internal and External Corners
Grooving of Floor
SHEET RUBBER
HEAT AND CHEMICAL WELDING
Page 12 of 17
http://www.american-biltrite.com | [email protected]
1-800-437-8743 6090-A (2019-05-21)
Welding of the Groove
SHEET RUBBER
HEAT AND CHEMICAL WELDING
Page 13 of 17
http://www.american-biltrite.com | [email protected]
1-800-437-8743 6090-A (2019-05-21)
Shaving of the Weld
Final Shaving
SHEET RUBBER
HEAT AND CHEMICAL WELDING
Page 14 of 17
http://www.american-biltrite.com | [email protected]
1-800-437-8743 6090-A (2019-05-21)
Chemical Welding of Sheet Rubber
Make Sure the Cut is Straight and Perfectly Perpendicular
Lightly Apply the Chemical Weld Product
SHEET RUBBER
HEAT AND CHEMICAL WELDING
Page 15 of 17
http://www.american-biltrite.com | [email protected]
1-800-437-8743 6090-A (2019-05-21)
Lay the Other Strip Close to the Other Piece Very Carefully
Wipe the Seam with a Damp Cleaned Rag
SHEET RUBBER
HEAT AND CHEMICAL WELDING
Page 16 of 17
http://www.american-biltrite.com | [email protected]
1-800-437-8743 6090-A (2019-05-21)
General Information
When ready to shave the hot weld strip, we suggest you use a soapy solution that you will apply on top of the lukewarm strip to shave off (the seam) then shave off the excess rod (use a good quality liquid dish washing soap, one cap in a gallon of water).
We suggest you use a 5mm speed tip. Tip side view
Tip top View
SHEET RUBBER
HEAT AND CHEMICAL WELDING
Page 17 of 17
http://www.american-biltrite.com | [email protected]
1-800-437-8743 6090-A (2019-05-21)
Heat Gun
Please note that technical web site documents prevail.