1
LAB REPORT DATE : 08/02/2012 Costumer: Mulag Articl e Comparazione grano austenitico tempra calore residuo – forno a tappeto Report 30MnCrB 5 Quenching from residual heat T= 960 °C Etchant: Oxalic acid 500 X Gsize : 6/7 30MnCrB 5 Quenching in mesh-belt furnace to water T= 860 °C Etchant: Oxalic acid 500 X Gsize : 9/10

Gsize boron steel

Embed Size (px)

DESCRIPTION

quenched from 960°Cquenched From 860°C

Citation preview

LAB

REPORTDATE : 08/02/2012Costumer:

Mulag

Article

Comparazione grano austenitico tempra calore residuo forno a tappeto

Report

30MnCrB 5

Quenching from residual heat

T= 960 C

Etchant: Oxalic acid500 X

Gsize : 6/7

30MnCrB 5

Quenching in mesh-belt furnace to waterT= 860 C

Etchant: Oxalic acid500 X

Gsize : 9/10