ChemInform 2011, 42, issue 21 © 2011 Wiley-VCH Verlag GmbH & Co. KGaA, Weinheim Lanthanoids I 2800 DOI: 10.1002/chin.201121008 Uniform Hollow Lu 2 O 3 :Ln (Ln: Eu 3+ , Tb 3+ ) Spheres: Facile Synthesis and Lumi- nescent Properties. — Carbon microspheres are hydrothermally obtained from aque- ous solutions of glucose (autoclave, 170 °C, 9 h) and used as templates in the synthesis of uniform hollow Lu2O3:Ln (Ln: Eu 3+ , Tb 3+ ) spheres by reaction of Lu(NO3)3 and Ln(NO3)3 in the presence of urea (H2O, 90 °C, 4 h; calcination in air, 800 °C, 2 h). The samples are characterized by XRD, SEM, TEM, UV/VIS diffuse reflectance, photolu- minescence, and cathodoluminescence spectroscopy. The as-prepared phosphors have diameters of about 300 nm and shell thicknesses of approximate 20 nm. Upon UV and low-voltage electron beam excitation, the materials exhibit bright red (Eu 3+ ) and green (Tb 3+ ) luminescence, which may find potential applications in the fields of color display and biomedicine. The synthesis method is suitable for inexpensive mass production of the hollow Lu2O3:Ln phosphors. — (YANG, P.; GAI, S.; LIU, Y.; WANG, W.; LI, C.; LIN*, J.; Inorg. Chem. 50 (2011) 6, 2182-2190, http://dx.doi.org/10.1021/ic101605k ; Key Lab. Superlight Mater. Surf. Technol., Harbin Eng. Univ., Harbin 150001, Peop. Rep. China; Eng.) — W. Pewestorf 21- 008

ChemInform Abstract: Uniform Hollow Lu2O3:Ln (Ln: Eu3+, Tb3+) Spheres: Facile Synthesis and Luminescent Properties

Embed Size (px)

Citation preview

Page 1: ChemInform Abstract: Uniform Hollow Lu2O3:Ln (Ln: Eu3+, Tb3+) Spheres: Facile Synthesis and Luminescent Properties

LanthanoidsI 2800 DOI: 10.1002/chin.201121008

Uniform Hollow Lu2O3:Ln (Ln: Eu3+, Tb3+) Spheres: Facile Synthesis and Lumi-nescent Properties. — Carbon microspheres are hydrothermally obtained from aque-ous solutions of glucose (autoclave, 170 °C, 9 h) and used as templates in the synthesis of uniform hollow Lu2O3:Ln (Ln: Eu3+, Tb3+) spheres by reaction of Lu(NO3)3 and Ln(NO3)3 in the presence of urea (H2O, 90 °C, 4 h; calcination in air, 800 °C, 2 h). The samples are characterized by XRD, SEM, TEM, UV/VIS diffuse reflectance, photolu-minescence, and cathodoluminescence spectroscopy. The as-prepared phosphors have diameters of about 300 nm and shell thicknesses of approximate 20 nm. Upon UV and low-voltage electron beam excitation, the materials exhibit bright red (Eu3+) and green (Tb3+) luminescence, which may find potential applications in the fields of color display and biomedicine. The synthesis method is suitable for inexpensive mass production of the hollow Lu2O3:Ln phosphors. — (YANG, P.; GAI, S.; LIU, Y.; WANG, W.; LI, C.; LIN*, J.; Inorg. Chem. 50 (2011) 6, 2182-2190, http://dx.doi.org/10.1021/ic101605k ; Key Lab. Superlight Mater. Surf. Technol., Harbin Eng. Univ., Harbin 150001, Peop. Rep. China; Eng.) — W. Pewestorf

21- 008

ChemInform 2011, 42, issue 21 © 2011 Wiley-VCH Verlag GmbH & Co. KGaA, Weinheim